Plasma in spark plasma sintering of ceramic particle compacts

Marder, Rachel and Estournès, Claude and Chevallier, Geoffroy and Chaim, Rachman Plasma in spark plasma sintering of ceramic particle compacts. (2014) Scripta Materialia, 82. 57-60. ISSN 1359-6462

[img]
Preview
(Document in English)

PDF (Author's version) - Requires a PDF viewer such as GSview, Xpdf or Adobe Acrobat Reader
226kB

Official URL: http://dx.doi.org/10.1016/j.scriptamat.2014.03.023

Abstract

Cuboidal LiF microcrystal powder was densified by spark plasma sintering at different pressures up to 500 °C. Densification at pressures above the yield stress occurred by plastic deformation and strain hardening. Densification at 2 MPa, below the yield stress, occurred by particle rearrangement assisted by viscous flow at the particle surfaces. Scanning electron microscopy examination of the fracture surfaces of the partially dense specimens revealed partial melting of the particle surfaces due to the plasma. The onset temperature for plasma formation was ∼180 °C.

Item Type:Article
Additional Information:Thanks to Elsevier editor. The definitive version is available at http://www.sciencedirect.com The original PDF of the article can be found at Scripta Materialia website : http://www.sciencedirect.com/science/article/pii/S1359646214001328
HAL Id:hal-01130774
Audience (journal):International peer-reviewed journal
Uncontrolled Keywords:
Institution:French research institutions > Centre National de la Recherche Scientifique - CNRS (FRANCE)
Université de Toulouse > Institut National Polytechnique de Toulouse - INPT (FRANCE)
Other partners > Technion – Israel Institute of Technology (ISRAEL)
Université de Toulouse > Université Toulouse III - Paul Sabatier - UPS (FRANCE)
Laboratory name:
Statistics:download
Deposited By: cirimat webmestre
Deposited On:12 Mar 2015 11:29

Repository Staff Only: item control page